PRODUCTS
PRODUCTS
Tension leveling line
Category:
E-mail:
Whatsapp:
-
Product Description
Many deep processing products are required to strip/coil surface has high straightness, if not through stretch bending straightening, removing grease, removing surface impurities such as aluminum powder, it is difficult meeting the user requirements simply through cold rolling mill.
Roller is deformed due to certain factors after the billet produced by hot rolled or roll casting process through cold rolling mill , which make the longitudinal extension in the width direction be not uniform , resulting in the wave of the aluminum belt. In order to eliminate the defects of the surface and slabs produced in the process of cold rolling, the aluminum strip after cold rolling must be cleaned and straightened.
Parameter
Aluminum Alloy 1000、3000、5000、8000Series Dia. of Drawing Roll 550--1300mm Rolling Speed 80--600m/min Entry Thickness 0.1--4.0mm Cleaning Mode Water clean Entry Width 600--2350mm Max. Extension Rate 4% Max.Weight of Coil Max 28000Kg Process Flow

APPLICATION
Tension levelers level and improve the flatness of materials such as hot rolled steel, cold rolled steel, stainless steel, aluminum, copper and specialized materials, and finish them into a final product.
MODEL TYPE
• Φ600×1250
• Φ800×1450
• Φ900×1650
• Φ1000×1850
• Φ1100×2000
• Φ1300×2300
• Φ1300×2800
Advantages
1. lmprove the flatness
2. lmprove the material anisotropy
3. Eliminate stress and prevent the formation of slip lines .
-
Many deep processing products are required to strip/coil surface has high straightness, if not through stretch bending straightening, removing grease, removing surface impurities such as aluminum powder, it is difficult meeting the user requirements simply through cold rolling mill.
Roller is deformed due to certain factors after the billet produced by hot rolled or roll casting process through cold rolling mill , which make the longitudinal extension in the width direction be not uniform , resulting in the wave of the aluminum belt. In order to eliminate the defects of the surface and slabs produced in the process of cold rolling, the aluminum strip after cold rolling must be cleaned and straightened.